Suitability of heat treatment for crack resistance of material in the connection part of heavy transporter for liquid slag (CROSBI ID 197072)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Vuherer, Tomaž ; Zrilić, M. ; Milović, Lj. ; Samardžić, Ivan ; Gliha, V. Suitability of heat treatment for crack resistance of material in the connection part of heavy transporter for liquid slag // Metalurgija, 53 (2013), 2; 243-246

Podaci o odgovornosti

Vuherer, Tomaž ; Zrilić, M. ; Milović, Lj. ; Samardžić, Ivan ; Gliha, V.

engleski

Suitability of heat treatment for crack resistance of material in the connection part of heavy transporter for liquid slag

The post weld heat treatment (PWHT) was used to reduce the level of the residual stresses and increase of the crack resistance of the material in the connection part. The article presents the results of the residual stress measurements immediately after welding and after the stress relaxation by the PWHT.

weld ; heat treatment ; residual stress ; stress relaxation ; crack resistance

Rad/časopis indeksiran je i u bazana: Advanced Technologies Database with AerospaceAerospace Database ; Aluminium Industry Abstracts ; ANTE ; Civil Engineering Abstracts ; Computer and Information Systems Abstracts (Module) ; Copper Technical Reference Library ; Corrosion Abstracts ; Earthquake Engineering Abstracts ; Electronics & ; Engineering Research Database ; Materials Business File ; Mechanical & Transportation Engineering Abstracts ; Solid State and Superconductivity Abstracts i Weldasearch.

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

53 (2)

2013.