Analysis of Austenitic Stainless Steels (AISI 303 and AISI 316Ti) Regarding Crack Driving Forces and Creep Responses (CROSBI ID 213378)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Vukelić, Goran ; Brnić, Josip Analysis of Austenitic Stainless Steels (AISI 303 and AISI 316Ti) Regarding Crack Driving Forces and Creep Responses // Proceedings of the institution of mechanical engineers part l-journal of materials-design and applications, 230 (2016), 3; 699-704. doi: 10.1177/1464420714565635

Podaci o odgovornosti

Vukelić, Goran ; Brnić, Josip

engleski

Analysis of Austenitic Stainless Steels (AISI 303 and AISI 316Ti) Regarding Crack Driving Forces and Creep Responses

Two types of austenitic stainless steels, AISI 303 and AISI 316Ti, were investigated experimentally and numerically in this paper in order to determine some of the material characteristics important for material selection in engineering design process. Ultimate tensile strength, yield strength and modulus of elasticity for room and selected elevated temperatures have been experimentally obtained. Improved heat resistance of AISI 316Ti can be noticed when comparing yield and tensile strength values of mentioned materials. Also, a comparison of material creep responses for selected temperatures and stress levels is presented. It can be noticed that at the same relative stress level AISI 303 exhibits higher strain percentage than AISI 316Ti. Also, as the temperature rises, AISI 316Ti holds stable strain percentage growth when comparing to AISI 303.In addition, a numerical procedure of determining crack driving force is performed using J-integral as a measure. Obtained J values are plotted versus specimen crack growth size (Δa) for different specimen geometries (a/W) and for different specimen types. Higher resulting values of J-integral for AISI 303 than AISI 316Ti can be noted. Although this procedure differs from experimental analysis, results can be useful as fracture parameter in fracture toughness assessment.

fracture; AISI 303; AISI 316Ti; SENB specimen; DCT specimen

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

230 (3)

2016.

699-704

objavljeno

1464-4207

10.1177/1464420714565635

Povezanost rada

Brodogradnja, Strojarstvo, Temeljne tehničke znanosti