Static and dynamic axial crush performance of in-situ foam-filled tubes (CROSBI ID 215864)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Duarte, Isabel ; Vesenjak, Matej ; Krstulović-Opara, Lovre ; Ren, Zoran Static and dynamic axial crush performance of in-situ foam-filled tubes // Composite structures, 124 (2015), 128-139. doi: 10.1016/j.compstruct.2015.01.014

Podaci o odgovornosti

Duarte, Isabel ; Vesenjak, Matej ; Krstulović-Opara, Lovre ; Ren, Zoran

engleski

Static and dynamic axial crush performance of in-situ foam-filled tubes

The aim of this paper is to study the quasi-static and dynamic compressive crush performance of newly developed in-situ foam-filled tubes (FFTs) made of light aluminium alloys prepared by powder compact foaming technique. By this method, the aluminium alloy empty tube is filled with an aluminium alloy foam during its formation. An extruded precursor of aluminium alloy and titanium hydride powder (0.5 wt.%) has been used for this purpose. The axial mechanical crushing behaviour and the failure mechanisms were assessed by uniaxial compression tests coupled with infrared thermography. The axial crush performance of in-situ FFTs was compared with performance of the individual components (integral-skin foam and empty tubes) submitted to the same heat treatment used to prepare the FFTs. Results confirm that the in-situ FFTs have a more stable axial crush performance. The results also demonstrate that heat treated aluminium alloy structures ensure high ductility and very good crashworthiness since they deform without formation of cracks during compression, which is a pre-requisite for good and reliable crashworthiness behaviour.

Aluminium foam In-situ foam-filled tubes; Uniaxial compression behaviour; Deformation modes; Crashworthiness; Energy absorption

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

124

2015.

128-139

objavljeno

0263-8223

10.1016/j.compstruct.2015.01.014

Povezanost rada

Strojarstvo

Poveznice
Indeksiranost